Specimen Preparation Sample Aggregation State HELICAL ARRAY Vitrification Instrument FEI VITROBOT MARK IV Cryogen Name ETHANE Sample Vitrification Details
3D Reconstruction Reconstruction Method HELICAL Number of Particles 108623 Reported Resolution (Å) 2.96 Resolution Method FSC 0.143 CUT-OFF Other Details Refinement Type Symmetry Type HELICAL Axial Symmetry C6 Axial Rise 4.77 Angular Rotation -0.64
Map-Model Fitting and Refinement Id 1 Refinement Space Refinement Protocol Refinement Target Overall B Value Fitting Procedure Details
Data Acquisition Detector Type GATAN K3 BIOCONTINUUM (6k x 4k) Electron Dose (electrons/Å**2) 39.28839
Imaging Experiment 1 Date of Experiment Temperature (Kelvin) Microscope Model TFS KRIOS Minimum Defocus (nm) 500 Maximum Defocus (nm) 2500 Minimum Tilt Angle (degrees) Maximum Tilt Angle (degrees) Nominal CS Imaging Mode BRIGHT FIELD Specimen Holder Model FEI TITAN KRIOS AUTOGRID HOLDER Nominal Magnification Calibrated Magnification Source FIELD EMISSION GUN Acceleration Voltage (kV) 300 Imaging Details
EM Software Task Software Package Version IMAGE ACQUISITION SerialEM CTF CORRECTION MotionCorr2 MODEL FITTING Coot RECONSTRUCTION RELION 4.0